HLT 3500 | Two part Hybrid Thermal Gel

Harmonization Code : 3824.99.96.99 | Prepared binders for foundry moulds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included : Other : Other: Other

HLT 3500 | Two part Hybrid Thermal Gel

Main features

  • Blue + White
  • 3.5 Thermal Conductivity
  • 0.44 Thermal impedance

Product Description

Honeywell HLT 3500 is a two-part hybrid gel product, dispensable and thermally conductive, which offers long-term reliability and superior softness. It exhibits low contact resistance, minimal oil bleeding at high temperatures and has very low thermal impedance under pressure. A balanced solution for vertical mounting that requires high TC before we go into the upper end of the product line. The enhanced bonding force between the polymer base and the filler largely improves the thermally conductive gel oil separation issue in storage.  Prior to curing, the material maintains good thixotropic characteristics and low viscosity to be easily dispensed.

Related Product:

One-part hybrid gel does not requires curing, check HT3500. HT3500 shares the same thermal properties as HLT3500. However, some process properties are difference. Check the comparison  between one-part and two-part hybrid thermal gel. 

Key Features:

  • Low contact resistance, BLT 0.1mm~5mm (TI vs Pressure curve)
  • Easy to dispense (>100 g/min rate) and rework (with acetone, IPA or toluene)
  • High compressibility for low stress applications (Thickness vs Pressure table)
  • Long-term reliability, less oil separation, and low outgassing (<0.5%)
  • No pump out, slump out and cracking
  • Up to 200 °C applicable temperature

Typical Applications:

  • Consumer electronics - gaming systems, portable devices
  • Telecommunications equipment - routers, servers, memory modules, hard disk drives, solid state drives
  • Automotive and aerospace - EV battery, power modules, capacitor cooling, lighting, charging units, ADAS

Curing Schedule:

HLT3500 can be cured at either 18 hours @room temperature or 30 minutes @100°C. You can optimize curing parameters for your own application needs. Check HLT Application Note to know storage and dispensing suggestions.

Product Family

SOLSTICE HLT3500

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
White - Blue
Specific GravitySpecific Gravity
3.2
Thermal Properties
Thermal ConductivityThermal Conductivity
3.5 W/m.K
Thermal ImpedanceThermal Impedance
0.44 °C·cm²/W
Physical Properties
ViscosityViscosity
300,000 - 450,000 mPa.s

Additional Information

HLT3500 Thermal Performance

HLT 3500 exhibits great Thermal impedance the more pressure you apply. At least 10psi pressure is suggested while applying it. 

 

Additionally the oil bleeding is minimal. The test has been conducted by pasting a 25.4 x 25.4 x 1.5mm sample on A4 paper, either at Room temperature or at 125oC 

Comparison between one-part and two-part hybrid gel

The HT series is one-part hybrid gel, which is already fully cross-linked before being applied. It could save time in assembly process and has longer shelf life. The HLT series products are two-part hybrid gels that can be cured in short-time after two-component mixing at room temperature. HLT products are cured in place, thus have better adhesion to components and are suitable for both horizontal and vertical applications. In total, the two series products share similar thermal and electrical properties. 

 Advantages Of Thermal Hybrid Gels

 

 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers