MOLYKOTE TP-42

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE TP-42

Main features

  • 3,000 N Four-Ball Weld Load
  • Water-Resistant Grease Lubrication
  • Stick-Slip, Galling, and Corrosion Protection

Product Description

MOLYKOTE® TP-42 Paste is a light-beige, adhesive grease-paste for heavily loaded metallic sliding surfaces. Its mineral- and synthetic-oil carrier system combines lithium soap, solid lubricants, and an adhesion improver to support lubrication where water or metal-machining emulsions may be present. The NLGI Grade 2 paste is used primarily for chucks and clamping elements on metal-processing machines, as well as assembly, run-in, spindle, bearing, bushing, sleeve, slide, guide, and track applications. It provides high load-carrying capacity, resistance to washout, corrosion and galling protection, and stick-slip control.

Key features

  • High load-carrying capacity: Provides a typical four-ball weld load of 3,000 N and an Almen-Wieland OK load of 20,000 N.
  • High adhesion: Contains an adhesion improver to help retain the paste on metallic sliding surfaces.
  • Washout resistance: Resists removal by water and metal-machining emulsions.
  • Stick-slip control: Supports smoother movement in slow-speed sliding contacts.
  • Galling and wear protection: Protects highly loaded metallic contacts during sliding and adjustment.
  • Corrosion protection: Provides a typical SKF-Emcor corrosion rating of 0–1.

Applications / Suitable for

  • Chucks and clamping elements on metal-processing machines
  • Sliding surfaces exposed to high contact pressures
  • Machining spindles
  • Plain bearings, bushings, and sleeves
  • Slides, guides, and tracks
  • Assembly and run-in lubrication
Product Family

MOLYKOTE TP-42

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product TypeProduct Type
Adhesive grease-paste for metallic sliding contacts; NLGI 2
Specific GravitySpecific Gravity
1.19 g/mL at 20°C
Thermal Properties
Operating TemperatureOperating Temperature
−25°C to 250°C for the solid-lubricant system °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied characteristics and storage information for MOLYKOTE® TP-42 Paste. Values are not intended as specification limits.

Property Value Unit Method / condition
Product type Adhesive grease-paste — For metallic friction combinations
Carrier system Mineral oil and synthetic oil — Supplier-listed composition
Thickener Lithium soap — Supplier-listed composition
Solid lubricant system White solid lubricants — Specific solids not identified in the TDS
Color Light beige — Typical property
NLGI grade 2 — Supplier product classification
Unworked penetration 265–300 0.1 mm ISO 2137
Density 1.19 g/mL ISO 2811 at 20°C
Usable life 60 months Original unopened container stored at or below 20°C
Technical properties

After-application / in-service properties

Typical performance characteristics of the applied paste under the stated laboratory conditions.

Property Value Unit Method / condition
Service-temperature range −25 to 250 °C Thermal stability of the solid-lubricant system
Drop point 125 °C ISO 2176; not a maximum service-temperature rating
Four-ball weld load 3,000 N DIN 51350-4
Four-ball wear scar 0.9 mm DIN 51350-5 under 800 N load
Almen-Wieland OK load 20,000 N Friction force: 1,710 N
Coefficient of friction 0.09 µ Press-fit test
Water resistance 2-90 — DIN 51807-1, static water-resistance rating
Corrosion protection 0–1 — DIN 51802, SKF-Emcor degree of corrosion
Oil separation 1.5 % DIN 51817 standard test

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers