LORD 506

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LORD 506

Main features

  • 4 to 6-Minute Working Window
  • Flexible Cured Adhesive
  • Environmental Resistance Acrylic Bonding

Product Description

LORD® 506 Acrylic Adhesive is a fast-curing structural acrylic adhesive designed for use with LORD® Accelerator 17 or 19. The mixed system forms a semi-flexible bond to a wide range of thermoplastics, thermoset plastics and prepared metals while accommodating shock and sudden stress loading. It cures rapidly at room temperature and provides documented performance from -40°F to 300°F (-40°C to 149°C).

Key Features

  • Broad substrate adhesion to ABS, acrylic, polycarbonate, FRP, prepared metals, urethane, phenolic, polysulfone and vinyl.
  • Rapid room-temperature cure with a 4–6 minute working time and handling strength in 8–12 minutes at 75°F (24°C).
  • Semi-flexible cured system accommodates shock and sudden stress loading.
  • Environmental and temperature resistance from -40°F to 300°F (-40°C to 149°C), including resistance to moisture, weathering and indirect UV exposure.

Applications / Suitable for

  • Thermoplastic and thermoset plastic bonding
  • ABS, acrylic and polycarbonate assemblies
  • FRP, urethane, phenolic, polysulfone and vinyl bonding
  • Prepared metal-to-plastic assemblies
Product Family

LORD 506

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Colorless to Amber Liquid
DensityDensity
989 -1036 kg/m3
Physical Properties
ViscosityViscosity
20,000 - 70,000 mPa.s
Thermal Properties
Flash PointFlash Point
11 °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Typical properties of LORD® 506 Acrylic Adhesive and its mixed systems with LORD® Accelerator 17 or 19. Values are typical and are not intended for specification purposes.

Property Value Unit Method / Condition
Appearance Colorless to amber liquid — LORD 506 adhesive, typical
Viscosity 20,000–70,000 cP Brookfield HBT, Spindle 3, 5 rpm at 77°F (25°C)
Density 8.25–8.65
(989–1036)
lb/gal
(kg/m³)
LORD 506 adhesive, typical
Flash Point 53
(11)
°F
(°C)
Closed cup
Mix Ratio with Accelerator 17 10:1 by volume Adhesive to accelerator
Mix Ratio with Accelerator 19 or 19 Black 10:5 by volume Adhesive to accelerator
Solids Content 100 % Mixed adhesive system
Working Time 4–6 minutes At 75°F (24°C)
Time to Handling Strength 8–12 minutes At 75°F (24°C); dependent on ambient temperature and mass; established at 100 psi
Mixed Appearance Tan paste
Grey paste
— Tan with Accelerator 17 or off-white Accelerator 19; grey with Accelerator 19 Black
Shelf Life 6 months Below 80°F (27°C) in the original, unopened container; storage at 40–50°F (4–10°C) recommended
Technical Properties

After-Processing / Final-State Properties

Supported cured-state properties for LORD® 506 Acrylic Adhesive used with LORD® Accelerator 17 or 19. Final appearance depends on the selected accelerator.

Property Value Unit Method / Condition
Full Cure Time 24 hours At room temperature
Cured Appearance with Accelerator 17 Tan to green — Typical
Cured Appearance with Accelerator 19 Tan to green — Off-white accelerator configuration
Cured Appearance with Accelerator 19 Black Black — Typical
Service Temperature Range -40 to 300
(-40 to 149)
°F
(°C)
Documented system performance range

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers