LOCTITE SI 5470

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LOCTITE SI 5470

Main features

  • Dual-Cure Sealing Processing
  • Low-Modulus Cured Sealing
  • Strong Plastic/Metal Adhesion

Product Description

LOCTITE® SI 5470™ is a dual-cure UV and moisture-curing silicone gasket material engineered to create soft, flexible, low-modulus foam gaskets for sealing applications. The product contains mechanically mixed nitrogen gas that produces a closed-cell foam structure and provides excellent adhesion to both plastics and metals. Functional strength develops almost instantly upon UV exposure, while secondary moisture cure ensures complete curing in shadowed areas and continued property development over 72 hours.

Key Features & Benefits

  • Dual-cure UV and moisture silicone technology.
  • Creates a closed-cell foam gasket structure.
  • Fast UV cure with secondary moisture cure.
  • Soft, flexible, low-modulus sealing material.
  • Excellent adhesion to plastics and metals.
  • Functional strength develops almost immediately after UV exposure.
  • Service temperature range from -40°C to +150°C.

Recommended Applications

  • Foam-in-place gasketing.
  • Plastic enclosure sealing.
  • Metal housing sealing.
  • Environmental protection seals.
  • Serviceable gasket applications.
Product Family

LOCTITE SI 5470

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
White/pale yellow paste
Specific GravitySpecific Gravity
1.03

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Silicone — Dual-cure foam gasket system
Chemical Type Acetoxy Silicone — Foamed silicone formulation
Appearance White / Pale Yellow Paste — Uncured material
Components One Component with Nitrogen Gas — Mechanically mixed
Primary Cure Ultraviolet Light — Rapid cure mechanism
Secondary Cure Moisture — Shadow-area curing
Temperature Range -40 to +150 °C Service range
Specific Gravity 1.03 — 25°C
Extrusion Rate 155 g/min 0.62 MPa, 25°C
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Tack-Free Time 15 seconds ASTM C679, 70 mW/cm² @ 365 nm
UV Depth of Cure 12 mm 60 sec @ 70 mW/cm²
Shore Hardness 54 Durometer OO ISO 868
Elongation at Break 163 % ISO 37
Tensile Strength 0.3 N/mm² ISO 37
Compression Set (20% Deflection) 21 % 22 h @ 25°C
Compression Set (30% Deflection) 20 % 22 h @ 25°C
Compression Set (40% Deflection) 19 % 22 h @ 25°C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers