LOCTITE CAT 15

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

LOCTITE CAT 15

Main features

  • Liquid Polyamide Epoxy Hardener
  • Two-Hour Pot Life
  • 80 deg C Accelerated Cure

Product Description

LOCTITE® CAT 15™ is a liquid polyamide-based epoxy hardener designed for use with compatible LOCTITE STYCAST® epoxy encapsulation, casting and potting systems. The hardener provides room-temperature curing capability, adjustable flexibility, long working life and excellent chemical resistance. Its low-toxicity profile and wide mixing ratio tolerance make it suitable for electrical insulation, electronic encapsulation and industrial composite applications where flexible, durable epoxy systems are required.

Key Features & Benefits

  • Polyamide epoxy hardener for epoxy resin systems.
  • Room-temperature or accelerated heat cure capability.
  • Provides flexible and durable cured systems.
  • Long working and pot life.
  • Good chemical and environmental resistance.
  • Suitable for potting, encapsulation and casting applications.
  • Compatible with electronic and electrical insulation systems.

Recommended Applications

  • Electronic component encapsulation.
  • Electrical potting and insulation systems.
  • Epoxy casting and composite fabrication.
  • Industrial maintenance and repair compounds.
  • Applications requiring flexible epoxy performance.
Product Family

LOCTITE CAT 15

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Product Type Epoxy Hardener — LOCTITE CAT 15 CLR
Technology Polyamide Cure System — Epoxy curing agent
Appearance Amber Liquid — As supplied
Odor Odorless — Ambient conditions
Density 0.98 g/cm³ 20°C
pH 10 — 100% product at 20°C
Flash Point >150 °C Closed cup
Initial Boiling Point >200 °C Typical value
VOC Content <3 % 2010/75/EC
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Pot Life (Reference Data) 2 hours 100 g mass at 25°C
Recommended Room Temperature Cure 16 - 24 hours Typical epoxy system cure
Accelerated Heat Cure 2 hours 80°C
Continuous Service Temperature 90 °C Typical cured system
Intermittent Service Temperature 120 °C Typical cured system
Skin Sensitization Classification Category 1 — H317
Skin Corrosion Classification Category 1B — H314
Environmental Classification Aquatic Chronic 2 — H411
Bioaccumulation Concern vPvB Substance Present — Contains hydrogenated terphenyl

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers