DOWSIL RSN-0805

Main features

  • Decorative and Protective Coating Resin
  • Enhanced Coating Softness and Flexibility
  • Standalone or Blendable Resin Use

Product Description

DOWSIL™ RSN-0805 Resin is a silanol-functional silicone resin supplied as a 50% solids solution in xylene for formulating high-performance decorative and protective coatings. It is intended primarily for use with metallic pigments in maintenance paints, colored baking enamels, and decorative finishes. Formulations based on the resin are designed to provide softness, flexibility, and high-temperature performance up to 650°C (1200°F). The resin may be used alone or blended with DOWSIL™ RSN-0806 Resin to increase film hardness.

Key features

  • High-temperature performance: Supports coating formulations designed to perform at temperatures up to 650°C (1200°F).
  • Formulation flexibility: Enhances softness and flexibility in decorative and protective coating formulations.
  • Blend-compatible silicone resin: Can be used alone or blended with DOWSIL™ RSN-0806 Resin to increase film hardness.

Applications / Suitable for

  • Maintenance paints formulated primarily with metallic pigments
  • Colored baking enamels
  • Decorative and protective coating formulations
Product Family

DOWSIL RSN-0805

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific GravitySpecific Gravity
1.01
Physical Properties
ViscosityViscosity
100-190 mPa.s
Thermal Properties
Flash PointFlash Point
27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties. Values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Composition Silanol-functional resin supplied as a solvent solution — As supplied
Diluent Xylene — As supplied
Resin solids 50 weight % 1.5 g, 3 hours at 135°C (275°F)
Specific gravity 1.01 — Typical value
Volatile organic content (VOC) 503 (4.2) g/L (lb/gal) Typical value
Viscosity 125 cP At 25°C (77°F)
Flash point, Tag closed cup 27 (81) °C (°F) Tag closed cup
Theoretical residual silicon dioxide 48 % Theoretical value
Phenyl/methyl ratio 1.1/1.0 — Typical value
Degree of substitution 1.6 — Typical value
Usable life 36 months From date of production when stored in the original unopened container

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers