DOWSIL EA-9187L UV Conformal Coating

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DOWSIL EA-9187L UV Conformal Coating

Main features

  • One-Part Solvent-Free Silicone Coating
  • Shore A 17 Hardness
  • 20 kV/mm Dielectric Strength

Product Description

DOWSIL™ EA-9187L UV Silicone Conformal Coating is a one-part, translucent, no-added-solvent silicone conformal coating for protecting printed circuit board assemblies and sensitive electronic components. The medium-viscosity material can be applied by spraying or dipping and cures through exposure to atmospheric moisture at room temperature, with mild heat available to accelerate cure. After cure, it forms a soft, stress-relieving elastomer with electrical insulation properties. A UV indicator supports inspection of coating coverage, while UL recognition includes UL 94 V-0 flammability classification and evaluation under UL 746C.

Key features

  • No-added-solvent silicone system: One-part formulation avoids solvent addition and is supplied at a typical viscosity of 900 mPa·s.
  • Soft elastomer after cure: Typical Shore A hardness of 17 supports low-stress protection of electronic components and interconnections.
  • Inspection and flammability support: Contains a UV indicator and carries UL recognition, including UL 94 V-0 and UL 746C.

Applications / Suitable for

  • Environmental protection of printed circuit board assemblies
  • Corrosion protection of electronic assemblies
  • Dielectric protection of electronic components and circuitry
  • Thin-section encapsulation of sensitive components
Product Family

DOWSIL EA-9187L UV

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Technical Specifications

No specifications available.

Additional Information

DOWSIL™ EA-9187L UV Silicone Conformal Coating is a one-part, translucent, no-added-solvent silicone conformal coating for protecting printed circuit board assemblies and sensitive electronic components. The medium-viscosity material can be applied by spraying or dipping and cures through exposure to atmospheric moisture at room temperature, with mild heat available to accelerate cure. After cure, it forms a soft, stress-relieving elastomer with electrical insulation properties. A UV indicator supports inspection of coating coverage, while UL recognition includes UL 94 V-0 flammability classification and evaluation under UL 746C.

Key features

  • No-added-solvent silicone system: One-part formulation avoids solvent addition and is supplied at a typical viscosity of 900 mPa·s.
  • Soft elastomer after cure: Typical Shore A hardness of 17 supports low-stress protection of electronic components and interconnections.
  • Inspection and flammability support: Contains a UV indicator and carries UL recognition, including UL 94 V-0 and UL 746C.

Applications / Suitable for

  • Environmental protection of printed circuit board assemblies
  • Corrosion protection of electronic assemblies
  • Dielectric protection of electronic components and circuitry
  • Thin-section encapsulation of sensitive components
Technical properties

After-processing / final-state properties

Typical properties measured after cure. Values are not intended for preparing specifications and should not be used alone as design values.

Property Value Unit Method / condition
Specific gravity 0.98 — Cured
Durometer hardness 17 Shore A Cured
Tensile strength 0.44 MPa Cured
Elongation at break 165 % Cured
Unprimed lap-shear strength 0.31 MPa Glass substrate
Dielectric strength 20 kV/mm Cured
Volume resistivity 3 × 1015 ohm·cm Cured
Dielectric constant 2.8 — At 1 MHz

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers