DOWSIL 839

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

DOWSIL 839

Main features

  • One-Part No-Mix Sealing
  • Non-Sag Placement Control
  • Electronics Assembly and Module Sealing

Product Description

DOWSIL™ 839 Silicone Adhesive/Sealant is a one-part, translucent blue, non-flowing silicone adhesive and sealant for general-purpose electrical and electronic assembly. The moisture-cure material requires no mixing and cures at room temperature, with mild heat below 60°C (140°F) available to accelerate cure when appropriate. Its non-flowing consistency supports controlled application through automated or manual needle-dispensing systems. The product is suitable for sealing openings in modules and housings, stabilizing individual components, assembling components on printed wiring boards, and sealing around wired or electrical leads.

Key features

  • One-part moisture-cure system: Requires no mixing and cures at room temperature in the presence of atmospheric moisture.
  • Non-flowing consistency: Provides zero reported slump for controlled placement on components, modules, and housings.
  • Dispensing flexibility: Can be applied using automated or manual needle-dispensing systems.

Applications / Suitable for

  • Sealing openings in modules and housings
  • Adding mechanical stability to individual components
  • Assembly of components on printed wiring boards
  • Sealing in and around wired and electrical leads
  • Yoke assembly
Product Family

DOWSIL 839

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Tack-Free TimeTack-Free Time
35 minutes
Mechanical Properties
Peel StrengthPeel Strength
25.5 N/cm²

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Appearance and form Translucent blue, non-flowing adhesive — One-part moisture-cure material
Extrusion rate 179 g/min Test method and dispensing conditions not stated
Flow rate – slump 0 in / cm Reported in both inch and centimetre units
Tack-free time 35 minutes At 25°C

After-processing / final-state properties

Typical cured-property values are not intended for use in preparing specifications. Cure and specimen conditions were not stated in the source table.

Property Value Unit
Tensile strength 285 / 2 / 20 psi / MPa / kg/cm²
Durometer hardness 32 Shore A
Unprimed adhesion 37 ppi
Peel strength 25.5 N/cm²

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers