DOWSIL 3-6060

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

DOWSIL 3-6060

Main features

  • Improved Inhibition Resistance
  • Promotes Bonding to Most Plastics
  • Wipe, Dip, or Spray Application

Product Description

DOWSIL™ 3-6060 Prime Coat is a one-part, solvent-based silicone surface treatment formulated to improve inhibition resistance and promote bonding for selected addition-cure and peroxide-cure silicone materials. The clear-to-yellow liquid is suitable for most plastics, ceramics, composites, and metals. It is applied as a very light, even coating by wiping, dipping, or spraying, then allowed to react with atmospheric moisture before the silicone material is applied.

Key features

  • Improved inhibition resistance: Formulated to improve inhibition resistance when processing compatible addition-cure silicone products.
  • Broad substrate suitability: Supports bonding to most plastics, ceramics, composites, and metals.
  • Compatible silicone systems: Intended for use with selected two-part addition-cure and peroxide-cure silicone materials.
  • Multiple application methods: May be applied in a very light, even coat by wiping, dipping, or spraying.

Applications / Suitable for

  • Priming most plastics, ceramics, composites, and metals
  • Improving inhibition resistance for compatible addition-cure silicone products
  • Promoting adhesion of selected two-part addition-cure and peroxide-cure silicones
Product Family

DOWSIL 3-6060

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
liquid

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied and processing properties. Values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Product form One-part liquid prime coat — Dilute solution of silane coupling agents and other active ingredients
Color Clear to yellow — As supplied
Solvent MIBK — Methyl isobutyl ketone carrier solvent
Flash point, closed cup 15 (59) °C (°F) Dow Corning Corporate Test Method 0917, based on ASTM D 3278
Volatile organic content 780 g/L Typical value
Typical cure time 1–2 hours Room temperature and 20–90% relative humidity; lower temperature or humidity requires longer cure
Shelf life 12 months From date of manufacture; store below 32°C (90°F) and protect from moisture

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers