DOWSIL 236

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

DOWSIL 236

Main features

  • Durable, Dry-Surfaced Silicone Rubber Coating
  • Sticky-Material Adhesion Prevention
  • Multiple Application Methods

Product Description

DOWSIL™ 236 Dispersion Coating is a one-part silicone rubber dispersion designed to form a dry-surfaced, durable release and protective coating. Supplied as a low-viscosity white liquid, it cures at room temperature through reaction with atmospheric moisture to produce a tough, rubbery electrical-insulating layer. The coating can help prevent sticky materials from adhering to processing equipment, reduce buildup and cleanup, and protect surfaces from weathering and corrosion. It may be applied by spraying, brushing, dipping, roller coating, or stamp coating.

Key features

  • Durable silicone rubber coating: Cures from a low-viscosity liquid to a smooth, white, dry-surfaced rubber layer.
  • Release and surface protection: Helps release sticky materials, reduce process buildup, and protect surfaces from weathering and corrosion.
  • Room-temperature moisture cure: Oxime-cure formulation reacts with moisture vapor in the air without requiring high-temperature processing.
  • Flexible application options: Can be applied by spraying, brushing, dipping, roller coating, or stamp coating.
  • On-site application and repair: Can be applied or repaired without disassembling supported equipment.

Applications / Suitable for

  • Release coatings for rolls, conveyors, dryer flights, and molding operations
  • Protection of surfaces from weathering, corrosion, dirt, and sticky materials
  • Linings for plastic containers or vessels
  • Latex manufacturing, paint-spraying, and waste-handling equipment
  • Urethane and polyester molding operations
Product Family

DOWSIL 236

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
white
SolidsSolids
70 %
Specific GravitySpecific Gravity
1.64
Thermal Properties
Flash PointFlash Point
10-12 °C
Operating TemperatureOperating Temperature
-40 to 150 °C
Physical Properties
Tack-Free TimeTack-Free Time
120 minutes
ViscosityViscosity
675 mPa.s
Mechanical Properties
ElongationElongation
500 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied and processing properties. Values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Composition Solvent dispersion of one-part silicone rubber — As supplied
Color White — CTM 0176
Flash point 50–53 (10–12) °F (°C) CTM 0021A
Solids 70 % CTM 0010
Viscosity 675 centipoise CTM 0050; at 77°F (25°C)
Vehicle VM&P naphtha — As supplied
Tack-free drying time 2 hours CTM 0095; cured at 72°F (22°C) and 50% relative humidity
Skin-over time 85 minutes At 72°F (22°C) and 50% relative humidity
Cure time 24 hours 0.100-inch section at 72°F (22°C) and 50% relative humidity
Recommended dry-film thickness per application 4–18 mils Additional coats may be used; allow 2–4 hours of drying between layers at room temperature in a humid atmosphere
Shelf life 12 months From date of manufacture; store below 90°F (32°C) in a closed container
Technical properties

After-processing / final-state properties

Typical cured-material properties. Values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Tensile strength 325 psi CTM 0137A; cured material
Elongation 500 % CTM 0137A; cured material
Durometer 20 Shore A points CTM 0099; cured material
Specific gravity 1.64 — CTM 0022; at 77°F (25°C)
Approximate service temperature −40 to 300 (−40 to 150) °F (°C) Approximate service-temperature range

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers