COOLTHERM EP-343

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM EP-343

Main features

  • 1.1 W/(m K) Thermal Interface
  • 1 to 6 mil Spray Coats
  • 59 kV/mm Dielectric Strength

Product Description

CoolTherm® EP-343 Thermally Conductive Epoxy Conformal Coating is a two-component, dielectric epoxy coating recommended for printed circuit boards, semiconductors, and heat sink assemblies. The black, low-viscosity mixed material can be applied with conventional spray equipment at 1–6 mils per application. After the documented cure schedule, it provides a typical thermal conductivity of 1.1 W/m·K, high electrical insulation, and an operating temperature range of -65 to 130 °C. The cured coating also provides resistance to water and a variety of chemicals, along with edge coverage and hiding power in thin applications.

Key features

  • Thermally conductive dielectric coating: Provides a typical cured thermal conductivity of 1.1 W/m·K using the Hot Disc Transient Method, ISO 22007-2.
  • Low-viscosity spray application: The mixed material has a typical viscosity of 55 cP at 25 °C and can be sprayed at 1–6 mils per application.
  • Electrical and temperature performance: Provides a typical dielectric strength of 59 kV/mm at 0.003-inch thickness and supports operating temperatures from -65 to 130 °C.

Applications / Suitable for

  • Printed circuit board coating
  • Semiconductor coating
  • Heat sink assembly coating

:contentReference[oaicite:0]{index=0}

Product Family

COOLTHERM EP-343

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Resin: Black Liquid | Hardener: Amber Liquid | Mixed: Black Liquid
Physical Properties
Viscosity (Part A)Viscosity (Part A)
(Resin) 65 mPa.s
Viscosity (Part B)Viscosity (Part B)
(Hardener) 55 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
106 °C
Thermal ConductivityThermal Conductivity
1.1 W/m.K
Mechanical Properties
ElongationElongation
at break 1.9 %
Chemical Properties
Moisture absorptionMoisture absorption
10 days at 25°C 0.2 %
Electrical Properties
Dielectric StrengthDielectric Strength
59 kV/mm
Volume ResistivityVolume Resistivity
1 x 10^16 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the separate components and mixed coating before cure. Values are not intended for specification purposes.

Property Value Unit Method / condition
Appearance Black liquid / amber liquid / black liquid — EP-343 resin / EP-343 hardener / mixed material
Mix ratio 100:3.9 By weight EP-343 resin : EP-343 hardener; no dilution required
Viscosity 65 / 55 / 55 cP Resin / hardener / mixed material at 25 °C; test method not stated
Specific gravity 1.41 / 0.99 / 1.35 — Resin / hardener / mixed material; test conditions not stated
Working life 24 hours Mixed material at 25 °C
Recommended applied thickness 1–6 mil Spray-applied in one application; greater thicknesses require partial oven curing between coats
Shelf life 1 / 2 years Resin / hardener when stored at 25 °C in original, unopened containers

 

Technical properties

After-processing / final-state properties

Typical cured properties after an initial cure of 2 hours at 65 °C followed by a post-cure of 4 hours at 135 °C. Values are not intended for specification purposes.

Property Value Unit Method / condition
Thermal conductivity 1.1 W/m·K Hot Disc Transient Method, ISO 22007-2
Coefficient of linear thermal expansion 24 ppm/°C ASTM C864
Glass transition temperature 106 °C Test method not stated
Hardness 90 Shore D Test method not stated
Tensile strength 57.22 (8,300) MPa (psi) Test method not stated
Moisture absorption 0.2 % 10 days at 25 °C; exposure medium not stated
Volume resistivity 1 × 1016 ohm-cm ASTM D257 at 25 °C
Dielectric strength 59 (1,500) kV/mm (V/mil) 0.003-inch specimen thickness; ASTM D149

 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers