BOSTIK LADH1531AC

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

BOSTIK LADH1531AC

Main features

  • Sprayable neoprene contact adhesive
  • Excellent green strength
  • High water, oil & heat resistance

Product Description

Bostik LADH1531AC is a solvent-based neoprene contact adhesive designed for high-speed spray application in veneer bonding and other industrial laminating processes. The sprayable formulation delivers excellent green strength for immediate handling while providing high water, oil, and heat resistance after bonding. It is formulated for large-area, uniform adhesive coverage, enabling rapid processing and reduced production time in industrial manufacturing environments. :contentReference[oaicite:0]{index=0}

Key Features

  • Sprayable neoprene contact adhesive for rapid, uniform adhesive application.
  • Excellent green strength allows immediate handling after bonding.
  • High water, oil, and heat resistance for demanding industrial applications.
  • Designed for fast production with quick bond development for high-speed manufacturing.

Applications / Suitable For

  • Veneer bonding
  • Industrial laminating
  • High-speed spray bonding
  • Large-area contact bonding
  • General industrial assembly
Product Family

BOSTIK LADH1531AC

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Process MethodProcess Method
Solvent evaporation
Product TypeProduct Type
Solvent-based neoprene contact adhesive
Thermal Properties
Operating TemperatureOperating Temperature
Drying at 80°C °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Product type Neoprene solution contact adhesive — Sprayable solvent-based adhesive
Appearance Tan liquid — Typical physical property
Total solids 16 % Typical value
Viscosity 185 cP LVF #2 @ 60 rpm, 25°C
Density 6.7 lb/gal Typical value
Flash point (SCC) -22 (-30) °F (°C) Typical value
Shelf life 270 days (9 months) — Stored between 55–100°F (13–38°C)
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Dry adhesive coat weight 2–5 g/ft² Applied to both substrates
Recommended drying condition 80 °C 1–3 minutes in circulating air oven
Press pressure 7 (0.5) psi (kg/cm²) 10–15 seconds for contact bonds
Green strength Adequate for immediate handling — After recommended bonding process
Performance High water, oil and heat resistance — Supplier description

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers