BONDERITE M-ZN 880BONDERITE M-ZN 880

Main features

  • Adhesion-Promoting Surface Treatment
  • Multi-Metal Spray/Immersion Pretreatment
  • Pre-Phosphate Corrosion-Resistance Improvement

Product Description

BONDERITE® M-ZN 880 MU is a zinc phosphating process designed to produce dense, fine-grained phosphate conversion coatings on iron, steel, aluminum, zinc, and zinc alloy surfaces prior to painting. The process utilizes BONDERITE® M-AC ZN as the titanium-based conditioning pretreatment to refine phosphate crystal structure, resulting in improved paint adhesion, coating durability, and corrosion resistance for multi-metal production lines. :contentReference[oaicite:0]{index=0}

Key Features

  • Produces fine-grained phosphate coatings for improved paint performance.
  • Titanium-based conditioning pretreatment promotes dense phosphate crystal formation.
  • Suitable for iron, steel, aluminum, zinc, and zinc alloys.
  • Supports both spray and immersion processing.
  • Improves paint adhesion and corrosion resistance in multi-metal pretreatment lines.

Applications / Suitable for

  • Iron
  • Steel
  • Aluminum
  • Zinc and zinc alloys
  • Automotive pretreatment
  • Industrial paint pretreatment
  • Multi-metal phosphating lines
Product Family

BONDERITE M-ZN 880

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product TypeProduct Type
Zinc phosphate process component

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Surface treatment — Supplier classification
Product type Powdered conditioning agent — Supplier classification
Application Surface treatment — Supplier classification
Chemistry Titanium-containing conditioning pretreatment — Supplier description
Application methods Spray or immersion — Supplier recommendation
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Spray total titanium 7–10 ppm Recommended operating range
Spray filterable titanium 3–5 ppm Recommended operating range
Immersion total titanium 15–20 ppm Recommended operating range
Immersion filterable titanium 5–10 ppm Recommended operating range
Operating pH 8.5–9.5 — Working bath
Operating temperature <120 °F Maximum operating temperature
Minimum contact time 20 seconds Spray or immersion

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers