BONDERITE M-NT 5700

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE M-NT 5700

Main features

  • Chromium-Free Ready-to-Use Aluminum Pretreatment
  • Corrosion-Resistant Paint-Adhesion Conversion Layer
  • Controlled Temperature-pH-Time Processing

Product Description

BONDERITE® M-NT 5700 is a chromium-free conversion coating specifically formulated for aluminum and its alloys. Supplied as a ready-to-use product, it forms colorless or bluish/yellowish conversion layers that provide excellent paint adhesion and very good corrosion resistance. The process is designed for efficient aluminum pretreatment without requiring in-plant dilution.

Key Features

  • Chromium-free conversion coating for aluminum and aluminum alloys.
  • Ready-to-use formulation requiring no in-plant dilution.
  • Produces colorless or bluish/yellowish conversion layers.
  • Provides very good corrosion resistance and excellent paint adhesion.
  • Simple immersion process with DI water rinse and drying.

Applications / Suitable for

  • Aluminum
  • Aluminum alloys
  • Paint pretreatment
  • Chromium-free conversion coating
  • Industrial metal finishing
Product Family

BONDERITE M-NT 5700

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product TypeProduct Type
Nanoceramic conversion coating
Thermal Properties
Operating TemperatureOperating Temperature
Ambient °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Metal Pretreatment — Supplier classification
Product Type Coating — Supplier classification
Application Conversion coating — Supplier classification
Chemistry Chromium-free — Supplier description
Supply form Ready-to-use — No in-plant dilution required
Storage temperature 0–40 °C Recommended storage
Shelf life 12 months From date of manufacture
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Operating concentration 7.1 points Ready-to-use bath
Operating temperature 20–50 °C Recommended operating range
Treatment time 1–5 minutes Typical process
Operating pH 2.6–3.8 — Working bath
Conversion coating appearance Colorless or bluish/yellowish — On aluminum and aluminum alloys
Performance Very good corrosion resistance and excellent paint adhesion — Finished conversion coating

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers