BONDERITE M-CR 1600

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE M-CR 1600

Main features

  • Hexavalent Chromate Conversion Coating
  • Immersion or Spray Processing
  • MIL-DTL-81706A/BAC 5719 Approval

Product Description

BONDERITE® M-CR 1600 AERO is a concentrated, two-package liquid chromate conversion coating for aluminum and all aluminum alloys. The process produces a hexavalent chromate conversion coating ranging from light iridescent gold to gold-tan, providing excellent corrosion protection and a durable base for subsequent paint application. The product supports immersion and spray processing, contains no complex cyanides, and is approved for aerospace applications meeting MIL-DTL-81706A and BAC 5719 requirements. :contentReference[oaicite:0]{index=0}

Key Features

  • Concentrated two-package liquid for chromate conversion coating.
  • Produces a hexavalent chromate coating with a light iridescent gold to gold-tan finish.
  • Suitable for immersion and spray application.
  • Contains no complex cyanides.
  • Approved to MIL-DTL-81706A and BAC 5719 for aerospace surface treatment.

Applications / Suitable for

  • Aluminum and aluminum alloys
  • Aerospace conversion coating
  • Paint pretreatment
  • Corrosion protection
  • Immersion processing
  • Spray processing
Product Family

BONDERITE M-CR 1600

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product TypeProduct Type
Chromate conversion coating
Thermal Properties
Operating TemperatureOperating Temperature
Ambient °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Chromate conversion coating — Supplier classification
Product type Concentrated two-package liquid — As supplied
Chemistry Hexavalent chromate — Supplier description
Application methods Immersion, Spray — Supplier recommendation
Complex cyanides None — Supplier description
Qualified specifications MIL-DTL-81706A Class 1A & 3, Form I Method C; BAC 5719 — Supplier published
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Coating appearance Light iridescent gold to gold-tan — Typical finished coating
Performance Corrosion protection — Conversion coating
Paint adhesion Provides an excellent base for painting — Supplier published
Substrate Aluminum and aluminum alloys — Finished application

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers