BONDERITE M-CR 1001

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE M-CR 1001

Main features

  • Clear Aluminum Chromate Conversion Coating
  • Paint-Adhesion and Corrosion-Resistance Improvement
  • Spray or Immersion Application

Product Description

BONDERITE® M-CR 1001 AERO is a nonflammable, chromic acid-based conversion coating for aluminum and aluminum alloys. It produces a clear chromate conversion coating that becomes an integral part of the aluminum surface, providing an excellent substrate for paint adhesion while improving corrosion resistance. The coating is especially suited for applications where the natural silver-white appearance of aluminum is to be retained, either unpainted or beneath a clear finish.

Key Features

  • Chromic acid-based conversion coating for aluminum and its alloys.
  • Clear conversion coating preserves the natural silver-white aluminum appearance.
  • Provides excellent corrosion resistance and paint adhesion.
  • Suitable for spray and immersion processing.
  • Nonflammable formulation.

Applications / Suitable for

  • Aluminum and aluminum alloys
  • Paint pretreatment
  • Corrosion protection
  • Clear-finish aluminum components
  • Spray conversion coating
  • Immersion conversion coating
Product Family

BONDERITE M-CR 1001

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product TypeProduct Type
Chromate conversion coating
Thermal Properties
Operating TemperatureOperating Temperature
Room temperature to 100°F (38°C) °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Metal pretreatment — Supplier classification
Product type Chromic acid conversion coating — Supplier description
Chemistry Chromic acid based — Supplier description
Flammability Nonflammable — Supplier description
Application methods Spray and immersion — Supplier recommendation
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Spray dilution 2 parts product : 3 parts water — Working solution preparation
Immersion bath preparation 25 parts product : 75 parts water — Working solution preparation
Operating temperature Ambient to 38 °C Ambient to 100°F
Immersion time 2–5 minutes Supplier recommendation
Spray time 15–30 seconds Supplier recommendation
Coating appearance Clear — Retains silver-white aluminum finish
BONDERITE titration 17–18 mL Recommended operating range
Maximum drying temperature 60 °C 140°F peak metal temperature

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers