BIOACT EC-78

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BIOACT EC-78

Main features

  • RMA/No-Clean/Lead-Free Flux Removal
  • Low-Foaming Electronics Cleaning
  • Saponifier and Corrosion-Inhibitor Formulation

Product Description

BIOACT™ EC-78 Aqueous Batch Defluxer is a concentrated, inherently low-foaming aqueous cleaner formulated with water-dilutable solvents, specialty saponifiers, and corrosion inhibitors. Designed for extended cleaning cycles in batch spray-in-air equipment, it removes a broad range of solder-flux residues while helping protect electronic assembly surfaces. The formulation operates without added defoamers or anti-tarnishing agents and is typically used at concentrations of 5% to 25%.

Key features

  • Broad flux-residue removal: Formulated to remove RMA, no-clean, lead-free, and water-soluble solder-flux residues.
  • Inherently low foaming: Supports the high temperatures and extended spray cycles commonly used in batch washers.
  • Integrated corrosion protection: Contains corrosion inhibitors to help protect electronic assembly surfaces during cleaning.
  • No supplemental additives required: Does not require added defoamers or anti-tarnishing agents to maintain cleaning performance.

Applications / Suitable for

  • Aqueous batch spray-in-air cleaning equipment
  • Defluxing printed circuit board assemblies
  • Removal of RMA, no-clean, lead-free, and water-soluble flux residues
  • Extended-cycle batch washing processes
Product Family

BIOACT EC-78

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Flash PointFlash Point
None to boiling °C
General Properties
Specific GravitySpecific Gravity
0.944
Physical Properties
ViscosityViscosity
16 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied and recommended process properties. Values are not intended for use as specifications.

Property Value Unit Method / condition
Product type Concentrated aqueous batch defluxer — Water-dilutable formulation
Formulation Water-dilutable solvents, specialty saponifiers, and corrosion inhibitors — As supplied
Odor Mild — As supplied
Flash point None to boiling — Reported in the supplied TDS
Specific gravity 0.944 — At 25°C
Viscosity 16 cps At 25°C
pH 10.1 — 15% concentration
Recommended use concentration 5–25 % Batch spray-in-air cleaning
Recommended operating temperature 120–160 (50–70) °F (°C) Batch spray-in-air cleaning

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers