ABLESTIK FDA 22

Harmonization Code : 5906100000 | Adhesive tape of a width not exceeding 20cm

ABLESTIK FDA22

Main features

  • 1.50 x 10^14 ohm-cm Volume Resistivity
  • 3-Hour Working Window
  • 2,100 psi Aluminum Lap Shear

Product Description

LOCTITE® ABLESTIK FDA 22 is a two-part, electrically insulating epoxy adhesive for medical-device bonding and coating applications. The tan, high-viscosity system mixes at 100:40 by weight and provides a typical pot life of 3 hours. It can be cured for 24 hours at 25°C or accelerated for 1 to 4 hours at 65°C. The cured material has a documented operating-temperature range of -70 to 145°C, typical volume resistivity of 1.50 × 1014 ohm-cm at 25°C, and aluminum-to-aluminum lap shear strength of 2,100 psi.

Key features

  • Electrically insulating: Typical cured properties include volume resistivity of 1.50 × 1014 ohm-cm at 25°C and dielectric strength of 420 V/mil.
  • High-viscosity epoxy system: Mixed viscosity of 28,000 cP at 25°C supports controlled application in bonding and coating processes.
  • Room-temperature or heat cure: Guideline cure schedules include 24 hours at 25°C or 1 to 4 hours at 65°C.

Applications / Suitable for

  • Catheters
  • Hearing aids
  • Dental products
  • Other biomedical instruments and devices
  • Bonding and coating applications
Product Family

ABLESTIK FDA 22

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Tan
Chemistry TypeChemistry Type
Epoxy
Component SystemComponent System
Two part - Resin & Hardener
Mix RatioMix Ratio
100 : 40
Pot LifePot Life
3 hours
Specific GravitySpecific Gravity
1.45
Thermal Properties
Operating TemperatureOperating Temperature
-70 to 145 °C
Physical Properties
Thixotropic indexThixotropic index
1.2
Mechanical Properties
ElongationElongation
5 %
Electrical Properties
Volume ResistivityVolume Resistivity
1.5 x 10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties and processing characteristics of the two-part adhesive before cure.

Property Value Unit Method / condition
Technology Epoxy — Two-part resin and hardener system
Appearance Tan — Mixed adhesive
Mix ratio — resin:hardener 100:40 by weight Resin-to-hardener ratio
Mixed viscosity 28,000 cP At 25°C; method not stated
Thixotropic index 1.2 — 5/50 rpm
Specific gravity — mixed 1.45 — Mixed adhesive
Reactive solids content 100 % Typical value
Pot life 3 hours Test conditions and endpoint not stated
Cure schedule 24 hours or 1–4 hours — 24 hours at 25°C or 1–4 hours at 65°C; guideline recommendations
Optimal storage 27 °C Store unopened in a dry location; package labeling governs applicable storage information
Technical properties

After-processing / final-state properties

Typical properties and performance data for the cured adhesive. Values are reference data and are not product specifications.

Property Value Unit Method / condition
Operating-temperature range -70 to 145 °C Documented product range
Coefficient of thermal expansion 47 ppm/°C Method, temperature region, and cure condition not stated
Hardness 78 Shore D Method and cure condition not stated
Elongation 5 % Method and cure condition not stated
Volume resistivity at 25°C 1.50 × 1014 ohm-cm Test method and specimen configuration not stated
Dielectric strength 420 V/mil Test method, thickness, and conditioning not stated
Dielectric constant 3.5 — At 25°C and 1 kHz
Dissipation factor 0.02 — At 25°C and 1 kHz
Lap shear strength — aluminum to aluminum 2,100 psi Substrate preparation, bondline, cure condition, test method, and test temperature not stated

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers